“Which films can your machine run?” is a common question. We can configure equipment for a range of films. The choice starts with your product. A clear overwrap on a gift box, a film that must hold a case of bottles together, and a wrap that must protect chocolate from heat solve different problems. First agree what the film needs to do. Then check whether a specific grade will feed, seal and shrink on the proposed equipment.
Choose candidates by what the pack has to do
| What you are packaging | Film worth trying first | What could change the choice |
|---|---|---|
| Printed cartons, cards or gift boxes | Clear POF (polyolefin) overwrap. Compare haze and the finished seam. | Light cartons or thin trays can bow if the film pulls too hard. Test a lower-shrink-force grade. Check printed faces and corners after cooling. [2] |
| Bottle or can multipacks carried as a unit | PE (polyethylene) collation shrink film. Compare grade, gauge and sealing performance under the actual load. | Check the pack after cooling and after lifting, stacking or conveying it as intended. A strong film can still lose the pack through a weak seam or a puncture at a tray edge. [3] |
| Contoured bottle with a printed decorative label | A shrink-sleeve grade such as PETG, or a suitable PVC sleeve grade where the specification and market allow it. | Ask for shrink across and along the roll. Check artwork distortion and whether the finished bottle and label can be sorted and recycled in the destination. This is a sleeve-label job with its own application and heat process. [4] [5] [7] |
| Chocolate or a product damaged by heat | Trial a low-temperature shrink grade in the required film family. Also ask whether the pack needs to shrink. | Confirm the product's heat limit, its temperature entering the tunnel, and the acceptable finished condition. If heat and acceptable shrink cannot be achieved together, consider a sealed outer wrap without a shrink step. [6] |
If the buyer already specifies PVC overwrap, qualify the actual grade and roll format on the intended sealer and check the destination requirements. The PVC sleeve example below is for a decorative label.
Tell the supplier whether the film is a retail finish, a restraint for grouped products, or a decorative sleeve. For a sharp-cornered pack ask for puncture and tear results as well as tensile strength. For a soft box ask for shrink force as well as shrink percentage. Low-temperature shrink and low shrink force solve different problems, and each needs its own check. [2] [3]
Read the numbers with the test conditions attached
Free shrink describes how much an unrestrained film specimen contracts. Ask for both directions, MD (along the roll) and TD (across it), plus temperature, exposure time and test medium. Shrink tension measures the force generated when contraction is restrained. A film with a large free-shrink value can still be a poor fit for a flimsy tray or a pack whose shape must be preserved. [1] [2]
| Material and sample | Reported result | Test conditions and source |
|---|---|---|
| Renolit TD 50P PVC sleeve film | <5% MD / 50 ± 2% TD | 95 °C, water, 30 s, DIN 53377, Rev. 6 data sheet. [5] |
| Transcendia SP690A PETG sleeve film | 48% TD at 70 °C and 72% TD at 80 °C | Each in a water bath for 10 s. The manufacturer reports TD for these conditions. [4] |
These are examples of specific grades and lab methods. The test conditions differ by grade. Compare candidates under matched conditions before ranking them. A water-bath result describes the specimen under that test and gives no production tunnel temperature or conveyor setting. Use a matched test to compare candidate films. Transfer the result to a production setting only after checking your packs in the actual tunnel.
To compare appearance at the same gauge, ask for haze and check how clearly the actual label or printing reads through the film. For mechanical performance, compare puncture or tear as appropriate, and verify seal strength separately. In its own collation-film test report, ExxonMobil compared specific formulations at the same 50 µm gauge and reported puncture, impact, tear and haze separately. The results apply to the tested films. That is a better purchasing question than asking whether PE is “stronger” in general. [3]
Chocolate is a heat-exposure problem
A Zhongfu customer making chocolate raised a specific problem. The chocolate was liable to soften or melt when heated during packaging. A low-temperature shrink film was the route considered for reducing heat exposure. The customer example identifies the constraint. It supplies no recorded product-temperature limit, tested settings or validated production outcome for this article.
In an independent study, Zarić and colleagues measured melting by differential scanning calorimetry. Reported peak temperatures for the four chocolate samples were 33.3–34.7 °C. Some melting began below those peaks. Set the allowable product temperature and exposure for the actual chocolate against the buyer's quality criteria. Treat the lab melting peak, product temperature measured during the trial and tunnel air setpoint as three separate values. [6]
Ask for the free-shrink results of the standard and low-temperature grades at the same film thickness, exposure time and test medium. Compare shrink along and across the roll at several temperatures. Then test the lowest heat exposure that gives an acceptable fit on the actual pack. [1]
In a line trial, use actual chocolate, with its normal primary packaging and worst credible incoming temperature. Record the film grade, tunnel setting and time in the heated zone. Measure the product temperature where damage is most likely and inspect surface marks, softening or deformation along with film fit and seal condition. Repeat at the required output and account for a stop or a restart where the line design allows. If good shrink still takes more heat than the product accepts, revisit whether the customer needs the tight finish or simply a closed overwrap.
Check the market and the complete package
Recycling. Ask where the pack is sold and who collects and sorts it. Check the complete package, including inks, labels, closures, adhesives and how the film is removed. For the EU, the Packaging and Packaging Waste Regulation sets recyclability requirements in Article 6. Confirm the provisions and dates applicable to the package and destination when qualifying the film. A resin name alone does not establish that the finished pack will be collected and recycled. [7]
Food contact. Start with the finished package and how it will be used. Check intended contact and whether food contact or migration from the film is reasonably foreseeable, including through other layers. Consider the food type, heating temperature and time, and storage conditions. For the EU, apply the scope in Article 1 of Regulation (EC) No 1935/2004 and check Regulation (EU) No 10/2011 as amended for plastics within its scope. For the US, check the FDA framework for components reasonably expected to migrate under the intended conditions of use. Request current documentation for the exact grade, layer structure and use as required in the destination market. An outer-wrap label or a resin name alone does not establish its regulatory status. [8] [9] [10]
What evidence makes a film worth buying?
- Agree what fails. Examples include a puncture at the corner, a warped tray, an unreadable label, a loose group after lifting, or a damaged heat-sensitive product. Test the most demanding packs before accepting an average one.
- Compare the grades on the line. Record grade, gauge, width, feed direction, seal settings, tunnel air settings, conveyor speed and product temperature where relevant. Inspect seams before the tunnel, appearance after cooling and pack handling after the next transfer. That separates sealing faults from shrink and handling faults.
- Test how forgiving the choice is. Compare a sustained run, a film change and a restart at the required output. Record rejects and what caused them. Check whether a small change in speed or product condition takes the pack outside your acceptance limits.
Which fault is hardest to live with on your line? A looser corner, a crushed carton or a multipack that shifts after it leaves the conveyor each changes what you should test first. Choose the main failure to rule out first, then compare the grades that can meet your other requirements. If the film looks good only under a narrow set of conditions, discuss whether to change the grade, adjust the equipment or revise the pack design before committing to production.
Prepare samples for a film trial. Bring the finished pack, candidate film if available, the maximum acceptable change in appearance after heating and your target output.
Related: Shrink tunnels · Food box and tray outer wrapping · Bottle and can multipacks
Sources and test methods
- ASTM D2732, unrestrained linear thermal shrinkage. Liu and Harrison measured shrinkage versus time for specific LDPE films in Polymer Engineering & Science (1988). ASTM method · Peer-reviewed LDPE study.
- ASTM D2838, shrink tension and orientation release stress. ASTM method.
- ExxonMobil, Exceed Tough+ collation shrink fact sheet, p. 2, matched-gauge formulations and test methods. Manufacturer test report (PDF).
- Transcendia, SP690A copolyester shrink-sleeve film, p. 1. Manufacturer data sheet (PDF).
- RENOLITSHRINK TD 50P, Rev. 6, pp. 1–2. Manufacturer data sheet (PDF).
- Zarić et al., Processes 2024, 12(12), 2810, §3.3 and Table 3. Peer-reviewed chocolate study.
- Regulation (EU) 2025/40 on packaging and packaging waste, Article 6. EUR-Lex.
- Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food. EUR-Lex.
- US FDA, determining the regulatory status of components of a food contact material. FDA guidance.
- Regulation (EC) No 1935/2004, Article 1, scope for food-contact materials and articles. EUR-Lex consolidated text (PDF).